Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 85.76 MPa @Strain 2.75 %, Temperature 90.0 °C |
12440 psi @Strain 2.75 %, Temperature 194 °F |
ISO 527 |
DuPont Performance Polymers Rynite® FR543 NC010 PET Rynite® FR543 NC010 is a flame retardant, 43% glass reinforced polyethylene terephthalate. Has a 155C temperature index that is equivalent to many thermosets. Recognized by UL as UL94V-0 at 0.8mm.. |
|||
Tensile Stress | 85.77 MPa @Strain 2.20 %, Temperature 150 °C |
12440 psi @Strain 2.20 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 |