Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 86.56 MPa @Strain 1.63 %, Temperature 90.0 °C |
12550 psi @Strain 1.63 %, Temperature 194 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G50HSLA BK039B Nylon 66
(Unverified Data**) 50% Glass Reinforced Heat Stabilized Polyamide 66 Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 86.51 MPa @Strain 1.59 %, Temperature 0.000 °C |
12550 psi @Strain 1.59 %, Temperature 32.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 54G15HSLR BK031 Polyphthalamide (PPA)
(Unverified Data**) 15% Glass Reinforced Toughened PPA High Performance Polyamide Zytel HTN54G15HSLR BK031 is a 15% glass reinforced toughened heat stabilized hydrolysis resistant high performance polyamide resin. It i.. |