Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Stress = 13620 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 93.92 MPa

@Strain 0.900 %,
Temperature 150 °C
13620 psi

@Strain 0.900 %,
Temperature 302 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® HTN 52G45HSL NC010 Polyphthalamide (PPA)
Zytel® HTN52G45HSL NC010 is a 45% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds. It is also a PPA resin.Information provide..
Tensile Stress 93.907 MPa

@Strain 1.70 %,
Temperature 0.000 °C
13620 psi

@Strain 1.70 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Sorona® 3015G NC010 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)&
15% Glass Reinforced Polytrimethylene Terephthalate with Resin Made from Bio-PDO Sorona 3015G NC010 is a 15% glass reinforced PTT resin containing 31% renewably sourced ingredients by weight (37% ba..
Tensile Stress 93.89 MPa

@Strain 1.01022 %,
Temperature 0.000 °C
13620 psi

@Strain 1.01022 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK615SF NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
30% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK615SF is a 30% glass fiber reinforced low viscosity polybutylene terephthalate for injecti..
Copyright © lookpolymers.com All Rights Reserved