Mechanical Properties Metric English Comments
Tensile Stress 137.8 MPa

@Strain 1.50 %,
Temperature -20.0 °C
19980 psi

@Strain 1.50 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK645FR NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK645FR is a flame retardant 30% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.7..