Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 95.38 MPa @Strain 0.630 %, Temperature 0.000 °C |
13830 psi @Strain 0.630 %, Temperature 32.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G50HSLA BK039B Nylon 66
(Unverified Data**) 50% Glass Reinforced Heat Stabilized Polyamide 66 Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 95.34 MPa @Strain 1.94 %, Temperature 40.0 °C |
13830 psi @Strain 1.94 %, Temperature 104 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 73G50HSLA BK416 Nylon 6
(Unverified Data**) 50% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G50HSLA BK416 is a 50% glass fiber reinforced heat stabilized lubricated polyamide 6 resin for injection molding. It has an excellent surface.. |