Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 143.2 MPa @Strain 1.33 %, Temperature 0.000 °C |
20770 psi @Strain 1.33 %, Temperature 32.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN FR52G30BL NC010 Polyphthalamide (PPA)
(Unverified Data**) 30% Glass Reinforced Flame Retardant PPA High Performance Polyamide Zytel HTNFR52G30BL NC010 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin that has been devel.. |
|||
Tensile Stress | 143.2 MPa @Strain 1.89 %, Temperature 0.000 °C |
20770 psi @Strain 1.89 %, Temperature 32.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS 32CG20HSL BK409 Nylon 610
(Unverified Data**) 20% Carbon/Glass Reinforced Renewably Sourced Polyamide 610 Information provided by DuPont Performance Polymers |