Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 145.58 MPa @Strain 1.98 %, Temperature 0.000 °C |
21115 psi @Strain 1.98 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® GW520CS NC010 Polyethylene Terephthalate (PET) 20% Glass Reinforced Flame Retardant Polyethylene Terephthalate with Improved Glow Wire Performance Rynite GW520CS NC010 is a 20% glass fiber reinforced flame retardant color stabilized modified pol.. |