Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 1.03 MPa @Strain 100 %, Temperature 23.0 °C |
149 psi @Strain 100 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ OM 6240-1 Thermoplastic Elastomer (TPE) Versaflex™ OM 6240-1 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Except.. |
|||
Tensile Stress | 1.03 MPa @Strain 100 % |
149 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® P2840 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 1.03 MPa @Strain 100 %, Temperature 23.0 °C |
149 psi @Strain 100 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynalloy™ 8900-30 Thermoplastic Elastomer (TPE) Dynalloy™ 8900-series is an innovative thermoplastic elastomer selection formulated to provide the injection molder with a product capable of overmolding and bonding to both low-density polyethylen.. |
|||
Tensile Stress | 1.03 MPa @Strain 100 %, Temperature 23.0 °C |
149 psi @Strain 100 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7736-1 Thermoplastic Elastomer (TPE) Dynaflex™ G7736-1 is a general purpose compound designed to provide easy processing and a good surface finish. - Good Aesthetics - Good Ozone/UV Stability - High Flow for Thin-Wall Parts - Overmold.. |
|||
Tensile Stress | 1.03 MPa @Strain 0.0700 %, Temperature 40.0 °C |
149 psi @Strain 0.0700 %, Temperature 104 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC1000 BK385 Nylon 1010 UV Stabilized Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1000 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 90% renewably sourced ingredient by weight... |