Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 15.17 MPa @Strain 1.00 %, Temperature 80.0 °C |
2200 psi @Strain 1.00 %, Temperature 176 °F |
ISO 11403-1/-2 |
DuPont Performance Polymers Delrin® 511P BK402 Acetal Homopolymer Delrin® 511P is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding(reduced warpage, less shrinkage, fewer voids).Information provided .. |
|||
Tensile Stress | 15.17 MPa @Strain 11.93 %, Temperature 150 °C |
2200 psi @Strain 11.93 %, Temperature 302 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 444AHS BK152 Nylon 66
(Unverified Data**) Toughened Heat Stabilized Polyamide 66 Zytel 444AHS is a toughened heat stabilized black polyamide 66 resin for injection molding. It is a high flow processing friendly material.Information provided.. |