Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 156.79 MPa @Strain 1.32 %, Temperature 40.0 °C |
22741 psi @Strain 1.32 %, Temperature 104 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 92G45DH2 BK083 Polyphthalamide (PPA) 35% Glass Reinforced PPA High Performance Polyamide with DuPont Zytel HTN92G45DH2 BK083 is a 45% glass reinforced high performance polyamide resin using DuPont SHIELD Technology with high flow and e.. |