Polymer Property : Tensile Stress = 1574 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 10.85 MPa

@Strain 7.37 %,
Temperature 100 °C
1574 psi

@Strain 7.37 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 8238 Polyester Elastomer TPC-ET  (Unverified Data**)
82 Shore D Standard Performance Polyester ElastomerInformation provided by DuPont Performance Polymers