Mechanical Properties Metric English Comments
Tensile Stress 16.1 MPa

@Strain 0.250 %,
Temperature 40.0 °C
2340 psi

@Strain 0.250 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK643FR NC010 Polybutylene Terephthalate (PBT)
20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK643FR is a flame retardant 20% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.8..
Tensile Stress 16.1 MPa

@Strain 6.00 %,
Temperature 150 °C
2340 psi

@Strain 6.00 %,
Temperature 302 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® E51HSB NC010 Nylon 66  (Unverified Data**)
Unreinforced Heat Stabilized High Viscosity Polyamide 66 Zytel E51HSB NC010 is a high molecular weight heat stabilized polyamide 66 resin for injection molding and extrusion.Information provided by ..
Tensile Stress 16.1 MPa

@Strain 5.00 %,
Temperature 0.000 °C
2340 psi

@Strain 5.00 %,
Temperature 32.0 °F
ISO 527
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET  (Unverified Data**)
Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac..