Mechanical Properties Metric English Comments
Tensile Stress 16.6 MPa

@Strain 0.210 %,
Temperature 60.0 °C
2410 psi

@Strain 0.210 %,
Temperature 140 °F
ISO 527
DuPont Performance Polymers Crastin® SK608 BK509 PBT  (Unverified Data**)
Crastin® SK608 BK509 is a 45% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Stress 16.6 MPa

@Strain 0.500 %,
Temperature 23.0 °C
2410 psi

@Strain 0.500 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 900P BK602 Acetal (POM)  (Unverified Data**)
Low Viscosity Acetal Homopolymer with Improved ProcessingDelrin 900P BK602 is a low viscosity black acetal homopolymer resin for multicavity and thin wall molding. It offers an improved processing t..
Tensile Stress 16.6 MPa

@Strain 30.38 %,
Temperature 90.0 °C
2410 psi

@Strain 30.38 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® ST820 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
Unreinforced Polybutylene Terephthalate with Excellent Impact Resistance Crastin ST820 NC010 is an unreinforced Super Tough polybutylene terephthalate resin for injection molding.Information provide..
Tensile Stress 16.6 MPa

@Strain 35.0 %,
Temperature 23.0 °C
2410 psi

@Strain 35.0 %,
Temperature 73.4 °F
ISO 527
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET  (Unverified Data**)
Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac..
Tensile Stress 16.6 MPa

@Strain 40.0 %,
Temperature 23.0 °C
2410 psi

@Strain 40.0 %,
Temperature 73.4 °F
ISO 527
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET  (Unverified Data**)
Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac..
Tensile Stress 16.6 MPa

@Strain 45.0 %,
Temperature 23.0 °C
2410 psi

@Strain 45.0 %,
Temperature 73.4 °F
ISO 527
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET  (Unverified Data**)
Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac..
Tensile Stress 16.6 MPa

@Strain 50.0 %,
Temperature 23.0 °C
2410 psi

@Strain 50.0 %,
Temperature 73.4 °F
ISO 527
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET  (Unverified Data**)
Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac..
Copyright © lookpolymers.com All Rights Reserved