Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 16.69 MPa @Strain 8.00 %, Temperature 90.0 °C |
2421 psi @Strain 8.00 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® ST830FRUV NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Flame Retardant UV Stabilized Polybutylene Terephthalate Crastin ST830FRUV NC010 is an unreinforced Super Tough flame retardant polybutylene terephthalate resin for injection molding. I.. |