Mechanical Properties Metric English Comments
Tensile Stress 11.04 MPa

@Strain 2.12 %,
Temperature 90.0 °C
1601 psi

@Strain 2.12 %,
Temperature 194 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6  (Unverified Data**)
Unreinforced Polyamide 6 Zytel 7335F NC010 is a nucleated lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Stress 11.04 MPa

@Strain 2.94 %,
Temperature 90.0 °C
1601 psi

@Strain 2.94 %,
Temperature 194 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS LC1000 BK385 Nylon 1010
UV Stabilized Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1000 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 90% renewably sourced ingredient by weight...