Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 112.8 MPa @Strain 1.40 %, Temperature -40.0 °C |
16360 psi @Strain 1.40 %, Temperature -40.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® IG38C1 BK434 Nylon 66
(Unverified Data**) 38% Mineral/Glass Reinforced Polyamide 66 Minlon IG38C1 BK434 is a 38% mineral/glass reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Performa.. |