Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 165 MPa @Strain 2.00 %, Temperature 0.000 °C |
23900 psi @Strain 2.00 %, Temperature 32.0 °F |
|
Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 Black 34 NG is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p.. |
|||
Tensile Stress | 165 MPa @Strain 2.00 %, Temperature 23.0 °C |
23900 psi @Strain 2.00 %, Temperature 73.4 °F |
|
Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 Black 34 NG is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p.. |
|||
Tensile Stress | 165 MPa @Strain 2.00 % |
23900 psi @Strain 2.00 % |
|
Solvay TECHNYL® A 218 V30 Black 21 NHFE PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 BLACK 21NHFE is a polyamide 6.6, high flow, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Be.. |
|||
Tensile Stress | 165 MPa @Strain 3.00 %, Temperature 80.0 °C |
23900 psi @Strain 3.00 %, Temperature 176 °F |
|
Solvay TECHNYLSTARâ„¢ AFX 218 V60 PA6, 60% glass filled, DRY Description: TECHNYLSTARâ„¢ AFX 218 V60 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 60% of glass fiber, for injection molding.Benefits: Due.. |
|||
Tensile Stress | 165 MPa @Strain 3.90 %, Temperature 40.0 °C |
23900 psi @Strain 3.90 %, Temperature 104 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G25HSL NC010 Nylon 66
(Unverified Data**) 25% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G25HSL NC010 is a 25% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perform.. |