Polymer Property : Tensile Stress = 16645 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 114.76 MPa

@Strain 2.74 %,
Temperature 23.0 °C
16645 psi

@Strain 2.74 %,
Temperature 73.4 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G35EF NC010 Nylon 66 + Nylon 6  (Unverified Data**)
35% Glass Reinforced Polyamide 66 Developed for Electrical and Electronics ApplicationsZytel 70G35EF NC010 is a 35% glass reinforced polyamide 66 developed for electrical and electronics application..
Tensile Stress 114.76 MPa

@Strain 2.74 %,
Temperature 23.0 °C
16645 psi

@Strain 2.74 %,
Temperature 73.4 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G35HSL NC010 Nylon 66  (Unverified Data**)
35% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G35HSL NC010 is a 35% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perform..