Mechanical Properties Metric English Comments
Tensile Stress 169.5 MPa

@Strain 2.80 %,
Temperature 90.0 °C
24580 psi

@Strain 2.80 %,
Temperature 194 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 51G35HSL NC010 Polyphthalamide (PPA)  (Unverified Data**)
35% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G35HSL NC010 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information ..