Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 17.92 MPa @Strain 5.00 %, Temperature 150 °C |
2599 psi @Strain 5.00 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 132F NC010 Nylon 66
(Unverified Data**) Unreinforced Nucleated Polyamide 66 Zytel 132F NC010 is a nucleated lubricated polyamide 66 for injection molding. It was developed for fast production cycles and high productivity applications.Info.. |