Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Stress = 17677 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 121.88 MPa

@Strain 1.13 %,
Temperature 0.000 °C
17677 psi

@Strain 1.13 %,
Temperature 32.0 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® PLS 93G35DH1 BK549 Nylon 6  (Unverified Data**)
35% Glass Reinforced Heat Stabilized Polyamide 6 Information provided by DuPont Performance Polymers