Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 18.5 MPa @Strain 0.520 %, Temperature 90.0 °C |
2680 psi @Strain 0.520 %, Temperature 194 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® 70G20HSL NC010 Nylon 66 Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 18.5 MPa @Strain 0.100 %, Temperature -40.0 °C |
2680 psi @Strain 0.100 %, Temperature -40.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 51G45HSL NC010 Polyphthalamide (PPA)
(Unverified Data**) 45% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G45HSL NC010 is a 45% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information .. |