Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 128.87 MPa @Strain 4.96 %, Temperature -40.0 °C |
18691 psi @Strain 4.96 %, Temperature -40.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 132F NC010 Nylon 66
(Unverified Data**) Unreinforced Nucleated Polyamide 66 Zytel 132F NC010 is a nucleated lubricated polyamide 66 for injection molding. It was developed for fast production cycles and high productivity applications.Info.. |