Mechanical Properties Metric English Comments
Tensile Stress 13.63 MPa

@Strain 0.430 %,
Temperature -40.0 °C
1977 psi

@Strain 0.430 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® 6129 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection MoldingInformation provided by DuPont Performance Polymers
Tensile Stress 13.63 MPa

@Strain 0.430 %,
Temperature -40.0 °C
1977 psi

@Strain 0.430 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® 6130 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)