Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 2.36 MPa @Strain 100 % |
342 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® P1765B TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 2.36 MPa @Strain 0.0400 %, Temperature 90.0 °C |
342 psi @Strain 0.0400 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 935SUV BK593 Polyethylene Terephthalate (PET)
(Unverified Data**) 35% Glass Reinforced UV Stabilized Polyethylene Terephthalate Rynite 935SUV BK593 is a 35% glass fiber /mineral reinforced UV stabilized modified polyethylene terephthalate resin with low warpage de.. |