Tensile Stress 2.69 MPa

@Strain 100 %,
Temperature 23.0 °C
390 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ HC MT307 Thermoplastic Elastomer (TPE)
Versaflex™ HC MT307 is an extrudable, autoclavable TPE developed for medical tubing applications in healthcare. New Product. Commercial specifications have not been established. - Autoclavable - Fl..
Tensile Stress 2.69 MPa

@Strain 100 %
390 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® P2665 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 2.69 MPa

@Strain 100 %
390 psi

@Strain 100 %
NEU NeuSoft™ 602-60A Ester TPU / SBC blend
Tensile Stress 2.69 MPa

@Strain 100 %,
Temperature 23.0 °C
390 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7410-1000-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G7410-1000-00 is an easy processing, high performance compound designed for use in applications requiring a tough, durable material. - Excellent Colorability - Excellent Heat Stability - ..
Tensile Stress 2.69 MPa

@Strain 100 %,
Temperature 23.0 °C
390 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7431-1001-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G7431-1001-00 is an easy processing, performance TPE designed for use in applications requiring a tough, durable material with a low coefficient of friction. - Excellent Heat Stability - ..
Tensile Stress 2.69 MPa

@Strain 100 %
390 psi

@Strain 100 %
510 mm/min; ASTM D412A
PolyOne Elastamax™ XL-2065 Thermoplastic Polyolefin Elastomer (TPO (POE))
PolyOne's Elastamax™ XL thermoplastic olefins (TPOs) are based on pelletized blends of polyolefin resins and select elastomers such EPDM. These materials have been engineered to provide a balance o..
Tensile Stress 2.69 MPa

@Strain 300 %,
Temperature 23.0 °C
390 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7702-9001-02 Thermoplastic Elastomer (TPE)
Dynaflex™ G7702-9001-02 is a performance TPE designed for a wide variety of applications. - Excellent Dimensional Stability - Excellent Heat Stability - High Resilience - Low Compression Set - Over..
Tensile Stress 2.69 MPa

@Strain 300 %
390 psi

@Strain 300 %
ASTM D412
Teknor Apex Telcar® TL-88-N873C BLK 111 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Tensile Stress 2.69 MPa

@Strain 149.53 %,
Temperature 120 °C
390 psi

@Strain 149.53 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4056 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 2.69 MPa

@Strain 6.08 %,
Temperature 40.0 °C
390 psi

@Strain 6.08 %,
Temperature 104 °F
ISO 527
DuPont Performance Polymers Hytrel® G4078W TPC-ET  (Unverified Data**)
Hytrel® G4078W is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like inject..