Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Stress = 2.70 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 2.70 MPa

@Strain 100 %
392 psi

@Strain 100 %
ISO 37
PolyOne OnFlex™ S FR 70A-3S1890 Thermoplastic Elastomer (TPE)
OnFlex™-S FR thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially flame retarded with a highly effective, RoHS compliant halo..
Tensile Stress 2.70 MPa

@Strain 0.000 %,
Temperature -20.0 °C
392 psi

@Strain 0.000 %,
Temperature -4.00 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS95G50DH2 BK261 Nylon  (Unverified Data**)
Zytel® PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology, only from DuPont providing exceptional Heat Resistance & High stiffness for automotive under hood..
Tensile Stress 2.70 MPa

@Strain 17.6 %,
Temperature 150 °C
392 psi

@Strain 17.6 %,
Temperature 302 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers
Tensile Stress 2.70 MPa

@Strain 300 %
392 psi

@Strain 300 %
ISO 37
Alliance Polymers Viprene™ G50A-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G50A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress 2.70 MPa

@Strain 300 %
392 psi

@Strain 300 %
ISO 37
Alliance Polymers Viprene™ G50A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G50A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress 2.70 MPa

@Strain 300 %
392 psi

@Strain 300 %
ISO 37
Alliance Polymers Viprene™ G50D-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G50D-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress 2.70 MPa

@Strain 300 %
392 psi

@Strain 300 %
ISO 37
Alliance Polymers Viprene™ G50D-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G50D-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress 2.70 MPa

@Strain 100 %
392 psi

@Strain 100 %
ISO 37
Alliance Polymers Viprene™ P70A-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ P70A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress 2.70 MPa

@Strain 100 %
392 psi

@Strain 100 %
ISO 37
Alliance Polymers Viprene™ P70A-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ P70A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..