Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 2.74 MPa @Strain 100 % |
397 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® C4660 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Tensile Stress | 2.74 MPa @Strain 16.71 %, Temperature 100 °C |
397 psi @Strain 16.71 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4068 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 2.74 MPa @Strain 32.19 %, Temperature 120 °C |
397 psi @Strain 32.19 %, Temperature 248 °F |
ISO 527 |
DuPont Performance Polymers Hytrel® G4078W TPC-ET
(Unverified Data**) Hytrel® G4078W is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like inject.. |