Mechanical Properties Metric English Comments
Tensile Stress 20.38 MPa

@Strain 0.500 %,
Temperature 100 °C
2956 psi

@Strain 0.500 %,
Temperature 212 °F
ISO 11403-1/-2
DuPont Performance Polymers Crastin® LW9330 BK851 PBT  (Unverified Data**)
Crastin® LW9330 BK851 is a 30% glass fiber reinforced, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional stability and low warp..
Tensile Stress 20.38 MPa

@Strain 2.20 %,
Temperature 100 °C
2956 psi

@Strain 2.20 %,
Temperature 212 °F
ISO 11403-1/-2
DuPont Performance Polymers Delrin® 511P BK402 Acetal Homopolymer
Delrin® 511P is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding(reduced warpage, less shrinkage, fewer voids).Information provided ..