Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 200 MPa

@Strain 2.00 %,
Temperature -40.0 °C
29000 psi

@Strain 2.00 %,
Temperature -40.0 °F
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, Conditioned
Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The ..
Tensile Stress 200 MPa

@Strain 2.00 %,
Temperature 0.000 °C
29000 psi

@Strain 2.00 %,
Temperature 32.0 °F
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, DRY
Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The ..
Tensile Stress 200 MPa

@Strain 1.00 %,
Temperature -40.0 °C
29000 psi

@Strain 1.00 %,
Temperature -40.0 °F
Solvay TECHNYLSTARâ„¢ AFX 218 V60 PA6, 60% glass filled, Conditioned
Description: TECHNYLSTARâ„¢ AFX 218 V60 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 60% of glass fiber, for injection molding.Benefits: Due..
Tensile Stress 200 MPa

@Strain 3.00 %,
Temperature 23.0 °C
29000 psi

@Strain 3.00 %,
Temperature 73.4 °F
Solvay TECHNYLSTARâ„¢ AFX 218 V60 PA6, 60% glass filled, Conditioned
Description: TECHNYLSTARâ„¢ AFX 218 V60 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 60% of glass fiber, for injection molding.Benefits: Due..
Tensile Stress 200 MPa

@Strain 1.00 %,
Temperature -40.0 °C
29000 psi

@Strain 1.00 %,
Temperature -40.0 °F
Solvay TECHNYLSTARâ„¢ AFX 218 V60 PA6, 60% glass filled, DRY
Description: TECHNYLSTARâ„¢ AFX 218 V60 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 60% of glass fiber, for injection molding.Benefits: Due..
Tensile Stress 200 MPa

@Strain 0.150 %
29000 psi

@Strain 0.150 %
Process Temperature T2
COI Ceramics Sylramic™ S300 Silicon Carbide Ceramic Matrix Composite, SiC
Description: Engineered ceramic composite structures for a broad range of industries and applications.Reinforcing Fiber Flexibility: S300 - Sylramic SiC Preceramic Polymer Matrix Precursors: S300 - ..
Tensile Stress 200 MPa

@Temperature 23.0 °C
29000 psi

@Temperature 73.4 °F
BASF Ultramid® Endure D3G7 Glass-Fiber Reinforced Polyamide
Description: Ultramid® Endure is a new, glass-fiber reinforced polyamide that combines excellent heat aging resistance with the good processing properties of PA 66. Ultramid® Endure can withstand ..
Tensile Stress 200 MPa

@Strain 3.00 %,
Temperature -40.0 °C
29000 psi

@Strain 3.00 %,
Temperature -40.0 °F
ISO 527
BASF Ultradur B 4300 G6 30% Glass Filled PBT
Ultradur B4300 G6 is an easy flowing injection molding PBT with 30% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small..