Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 140.43 MPa @Strain 1.34 %, Temperature 23.0 °C |
20368 psi @Strain 1.34 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN FR52G30BL NC010 Polyphthalamide (PPA)
(Unverified Data**) 30% Glass Reinforced Flame Retardant PPA High Performance Polyamide Zytel HTNFR52G30BL NC010 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin that has been devel.. |