Polymer Property : Tensile Stress = 205 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 205 MPa

@Strain 3.00 %
29700 psi

@Strain 3.00 %
Solvay TECHNYL® A 218 V35 Black 21NHFE PA66, 35% glass fiber, DRY
Description: TECHNYL® A 218 V35 BLACK 21NHFE is polyamide 6.6, high flow, reinforced with 35% glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits:..