Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 14.1 MPa @Strain 100 % |
2050 psi @Strain 100 % |
ISO 527-1/-2 |
DSM Arnitel® VT3108 TPC-ET Extrusion Grade, High Breathable, Drying of Material Required |
|||
Tensile Stress | 14.1 MPa @Strain 0.250 %, Temperature 90.0 °C |
2050 psi @Strain 0.250 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK645FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK645FR is a flame retardant 30% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.7.. |
|||
Tensile Stress | 14.1 MPa @Strain 50.0 %, Temperature 23.0 °C |
2050 psi @Strain 50.0 %, Temperature 73.4 °F |
ISO 527 (1BA bar) |
DuPont Performance Polymers Hytrel® HTR5612BK TPC-ET
(Unverified Data**) Hytrel® HTR5612BK HTR5612BK is designed for blow molding or processing techniques requiring high melt viscosity. It has nominal durometer hardness of 54D, is pigmented black with fine particle size.. |