Mechanical Properties Metric English Comments
Tensile Stress 208.47 MPa

@Strain 1.63 %,
Temperature -20.0 °C
30236 psi

@Strain 1.63 %,
Temperature -4.00 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® PLS 95G50DH2 BK261 Nylon 6  (Unverified Data**)
50% Glass Reinforced Heat Stabilized Polyamide Zytel PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology only from DuPont providing exceptional Heat Resistanc..