Polymer Property : Tensile Stress = 2126 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 14.66 MPa

@Strain 0.700 %,
Temperature 60.0 °C
2126 psi

@Strain 0.700 %,
Temperature 140 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® FR7026V0F NC010 Nylon 66  (Unverified Data**)
Zytel® FR7026V0F NC010 is a flame retardant, heat stabilized, polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by D..