Mechanical Properties Metric English Comments
Tensile Stress 148 MPa

@Strain 1.40 %,
Temperature 0.000 °C
21500 psi

@Strain 1.40 %,
Temperature 32.0 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G35HSLX BK357 Nylon 66  (Unverified Data**)
35% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G35HSLX BK357 is a 35% glass fiber reinforced heat stabilized black polyamide 66 for injection molding.Information provided by DuPont Perfor..
Tensile Stress 148 MPa

@Strain 0.100 %
21500 psi

@Strain 0.100 %
Process Temperature T2
COI Ceramics Sylramic™ S300 Silicon Carbide Ceramic Matrix Composite, SiC
Description: Engineered ceramic composite structures for a broad range of industries and applications.Reinforcing Fiber Flexibility: S300 - Sylramic SiC Preceramic Polymer Matrix Precursors: S300 - ..