Mechanical Properties Metric English Comments
Tensile Stress 1.55 MPa

@Strain 300 %,
Temperature 23.0 °C
225 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynalloy™ 8900-30 Thermoplastic Elastomer (TPE)
Dynalloy™ 8900-series is an innovative thermoplastic elastomer selection formulated to provide the injection molder with a product capable of overmolding and bonding to both low-density polyethylen..