Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 23.9 MPa @Strain 0.250 %, Temperature 23.0 °C |
3470 psi @Strain 0.250 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9030 NC010 PBT+ASA
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030 NC010 is a 30% glass fiber reinforced polybutylene terephthalate blend for injection molding. .. |
|||
Tensile Stress | 23.9 MPa @Strain 6.20 %, Temperature 90.0 °C |
3470 psi @Strain 6.20 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500AF Acetal (POM)
(Unverified Data**) 20% Teflon® Fiber Filled Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500AF is a medium viscosity acetal homopolymer resin containing 20% Teflon PTFE fibers. It is desi.. |
|||
Tensile Stress | 23.9 MPa @Strain 18.8 %, Temperature 150 °C |
3470 psi @Strain 18.8 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 103HSL NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 103HSL NC010 is a heat stabilized lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |