Polymer Property : Tensile Stress = 23055 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 158.96 MPa

@Strain 1.25 %,
Temperature 0.000 °C
23055 psi

@Strain 1.25 %,
Temperature 32.0 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G50HSLA BK039B Nylon 66  (Unverified Data**)
50% Glass Reinforced Heat Stabilized Polyamide 66 Information provided by DuPont Performance Polymers