Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 24.39 MPa @Strain 0.330 %, Temperature 150 °C |
3537 psi @Strain 0.330 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G50HSLA BK039B Nylon 66
(Unverified Data**) 50% Glass Reinforced Heat Stabilized Polyamide 66 Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 24.39 MPa @Strain 13.51 %, Temperature 90.0 °C |
3537 psi @Strain 13.51 %, Temperature 194 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 153HSL NC010 Nylon 612
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 612 Information provided by DuPont Performance Polymers |