Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 169.84 MPa @Strain 2.23 %, Temperature -20.0 °C |
24633 psi @Strain 2.23 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® HR5330HF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)& 30% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5330HF is a 30% glass reinforced PBT with high flow (HF) moderately toughened hydrolysis resistant (HR) resin. Excellen.. |