Tensile Stress 17.68 MPa

@Strain 1.70 %,
Temperature 80.0 °C
2564 psi

@Strain 1.70 %,
Temperature 176 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® FR7026V0F NC010 Nylon 66  (Unverified Data**)
Zytel® FR7026V0F NC010 is a flame retardant, heat stabilized, polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by D..
Tensile Stress 17.68 MPa

@Strain 0.500 %,
Temperature 150 °C
2564 psi

@Strain 0.500 %,
Temperature 302 °F
50%RH; ISO 11403-1/-2
DuPont Performance Polymers Zytel® HTN FR52G20NH BK337 Polyphthalamide (PPA)
Zytel® HTNFR52G20NH BK337 is a 20% glass reinforced, flame retardant, lubricated high performance polyamide resin. It is also a PPA resin and it uses a non-halogenated flame retardant.Information p..