Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 178 MPa

@Strain 2.00 %,
Temperature -30.0 °C
25800 psi

@Strain 2.00 %,
Temperature -22.0 °F
Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, DRY
Description: TECHNYL® A 218 V30 Black 34 NG is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p..