Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 26.3 MPa @Strain 1.50 %, Temperature 160 °C |
3810 psi @Strain 1.50 %, Temperature 320 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK643FR NC010 Polybutylene Terephthalate (PBT) 20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK643FR is a flame retardant 20% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.8.. |
|||
Tensile Stress | 26.3 MPa @Strain 15.0 %, Temperature 120 °C |
3810 psi @Strain 15.0 %, Temperature 248 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® E42A NC010 Nylon 66
(Unverified Data**) Zytel® E42A is a high viscosity polyamide 66 for injection molding and extrusion. It has improved break resistance for thick-walled parts.Information provided by DuPont Performance Polymers |