Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 26.5 MPa @Strain 11.0 %, Temperature 90.0 °C |
3840 psi @Strain 11.0 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500T NC010 Acetal (POM)
(Unverified Data**) Toughened Medium Viscosity Acetal Homopolymer Delrin 500T NC010 is a toughened medium viscosity acetal homopolymer resin with impact resistance similar to Delrin 100. It can be used in parts requiri.. |
|||
Tensile Stress | 26.5 MPa @Strain 1.20 %, Temperature 40.0 °C |
3840 psi @Strain 1.20 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG500P NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG500P is a medium viscosity acetal homopolymer with improved thermal stability. It has been developed for consider.. |
|||
Tensile Stress | 26.5 MPa @Strain 0.630 %, Temperature -20.0 °C |
3840 psi @Strain 0.630 %, Temperature -4.00 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 135F NC010 Nylon 66
(Unverified Data**) Unreinforced Nucleated Polyamide 66 Zytel 135F NC010 is a nucleated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Pe.. |