Tensile Stress 18.12 MPa

@Strain 0.300 %,
Temperature 60.0 °C
2628 psi

@Strain 0.300 %,
Temperature 140 °F
50%RH; ISO 11403-1/-2
DuPont Performance Polymers Zytel® HTN FR52G20NH BK337 Polyphthalamide (PPA)