Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 18.83 MPa @Strain 0.330 %, Temperature 150 °C |
2731 psi @Strain 0.330 %, Temperature 302 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN FR52G30BL NC010 Polyphthalamide (PPA)
(Unverified Data**) 30% Glass Reinforced Flame Retardant PPA High Performance Polyamide Zytel HTNFR52G30BL NC010 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin that has been devel.. |
|||
Tensile Stress | 18.83 MPa @Strain 4.90 %, Temperature 150 °C |
2731 psi @Strain 4.90 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 12T NC010 Nylon 66
(Unverified Data**) 36% Mineral Reinforced Toughened Polyamide 66 Minlon 12T NC010 is a 36% mineral reinforced toughened heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performan.. |