Tensile Stress 1.89 MPa

@Strain 100 %
274 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® C4750 TPE, Transparent
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf..
Tensile Stress >= 1.89 MPa

@Strain 100 %
>= 274 psi

@Strain 100 %
ASTM D412 Method A
Seals Eastern 5753 Fluorocarbon-Elastomer
Features:MIL-SpecFKM general serviceInformation provided by Seals Eastern.
Tensile Stress 1.89 MPa

@Strain 12.94 %,
Temperature 120 °C
274 psi

@Strain 12.94 %,
Temperature 248 °F
ISO 527
DuPont Performance Polymers Hytrel® G4078W TPC-ET  (Unverified Data**)
Hytrel® G4078W is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like inject..