Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 28.13 MPa

@Strain 0.225 %,
Temperature -40.0 °C
4080 psi

@Strain 0.225 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK645FR NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK645FR is a flame retardant 30% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.7..
Tensile Stress 28.13 MPa

@Strain 3.05 %,
Temperature 150 °C
4080 psi

@Strain 3.05 %,
Temperature 302 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 73G15L NC010 Nylon 6  (Unverified Data**)
15% Glass Reinforced Polyamide 6Zytel 73G15L NC010 is a 15% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers