Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 28.593 MPa @Strain 1.454 %, Temperature 100 °C |
4147.1 psi @Strain 1.454 %, Temperature 212 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 510GR NC000 Acetal Homopolymer
(Unverified Data**) Delrin® 510GR is a 10% glass reinforced acetal homopolymer for injection molding. It has high strength, stiffness, and high deflection temperature and excellent creep resistance.Information provide.. |